Aluminum, 336.0, permanent mold cast, T65 | Mechanical Properties

Mechanical Properties for Aluminum 336.0 (T65)

PropertyValue RangeUnit
Young’s Modulus72.5 – 75.5GPa
Specific Stiffness26.7 – 27.9MN·m/kg
Yield Strength (Elastic Limit)281 – 311MPa
Tensile Strength309 – 341MPa
Specific Strength103 – 115kN·m/kg
Elongation1 – 2% strain
Compressive Strength281 – 311MPa
Flexural Modulus73.5 – 76.5GPa
Flexural Strength (Modulus of Rupture)281 – 311MPa
Shear Modulus27.5 – 28.9GPa
Bulk Modulus68.8 – 78.7GPa
Poisson’s Ratio0.322 – 0.338–
Shape Factor24–
Hardness – Vickers135 – 150HV
Elastic Stored Energy (Springs)534 – 653kJ/m³
Fatigue Strength at 10⁷ Cycles134 – 143MPa
Fatigue Strength Model (Stress Range)125 – 153MPa