AISI 1137 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 1137 Water Quenched & Tempered at 425°C Overview

AISI 1137 water quenched tempered 425°C is AISI 1137 resulfurized medium carbon steel (UNS G11370) in the water quenched & tempered at 425°C condition. This AISI 1137 water quenched tempered 425°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 1137 conditions in our AISI 1137 yield, tensile and hardness comparison. See also the resulfurized free-machining steels comparison. Looking for AISI 1137 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1137 steel parts in-house and inspects them before shipment.

AISI 1137 Water Quenched & Tempered at 425°C Designation

AISI 1137
ConditionTempered at 425°C & water quenched
UNS numberG11370
US nameASTM G11370, ASTM 1137 Class A, ASTM 1137, AMS 5024, ~SAE 1138
JIS (Japanese) nameSUM41

AISI 1137 Water Quenched & Tempered at 425°C Typical uses

Heavy duty shafts, axles, crankshafts, couplings, used particularly where enhanced machinability is important.

AISI 1137 Water Quenched & Tempered at 425°C Composition detail

C (carbon)0.32–0.39%
Fe (iron)97.8–98.2%
Mn (manganese)1.35–1.65%
P (phosphorus)0–0.04%
S (sulfur)0.08–0.13%

AISI 1137 Water Quenched & Tempered at 425°C Physical properties

Density7.8–7.9g/cm3

AISI 1137 Water Quenched & Tempered at 425°C Mechanical properties

Young’s modulus200–215GPa
Specific stiffness25.5–27.4MN.m/kg
Yield strength (elastic limit)885–1090MPa
Tensile strength990–1220MPa
Specific strength113–139kN.m/kg
Elongation11–17% strain
Compressive strength885–1090MPa
Flexural modulus200–215GPa
Flexural strength (modulus of rupture)885–1090MPa
Shear modulus77–84GPa
Bulk modulus155–175GPa
Poisson’s ratio0.285–0.295 
Shape factor25
Hardness – Vickers280–350HV
Elastic stored energy (springs)1900–2840kJ/m3
Fatigue strength at 10^7 cycles425–491MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
371–563MPa

AISI 1137 Water Quenched & Tempered at 425°C Impact & fracture properties

Fracture toughness23–40MPa.m0.5
Toughness (G)2.71–7.27kJ/m2

AISI 1137 Water Quenched & Tempered at 425°C Thermal properties

Melting point1440–1510°C
Maximum service temperature327–352°C
Minimum service temperature-38–-8°C
Thermal conductivity47–53W/m.°C
Specific heat capacity440–500J/kg.°C
Thermal expansion coefficient12–13.5µstrain/°C
Thermal shock resistance329–421°C
Thermal distortion resistance3.61–4.26MW/m
Latent heat of fusion270–275kJ/kg

AISI 1137 Water Quenched & Tempered at 425°C Electrical properties

Electrical resistivity16–19µohm.cm
Electrical conductivity9.07–10.8%IACS
Galvanic potential-0.52–-0.44V

AISI 1137 Water Quenched & Tempered at 425°C Magnetic properties

Magnetic typeMagnetic

AISI 1137 Water Quenched & Tempered at 425°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5050–5240m/s
Mechanical loss coefficient (tan delta)3.6e-4–4.5e-4 

AISI 1137 Water Quenched & Tempered at 425°C Processing properties

Metal castingUnsuitable
Metal cold formingAcceptable
Metal hot formingAcceptable
Metal press formingAcceptable
Metal deep drawingLimited use
Machining speed18.9 m/min
Weldability
Notes: Preheating and post weld heat treatments may be required
Poor
Carbon equivalency0.545 – 0.665

AISI 1137 Water Quenched & Tempered at 425°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)
Notes: Aluminum bronze is the most suitable mating material to minimize galling.
Acceptable
FlammabilityNon-flammable

AISI 1137 Water Quenched & Tempered at 425°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; Other susceptible environments: Nitrate, hydroxide, carbonate, ammonia
Slightly susceptible

AISI 1137 Water Quenched & Tempered at 425°C Notes

AISI 1137 Water Quenched & Tempered at 425°C Warning
Free cutting’ steel – in common with all such steels, it is not recommended where welding is involved.
AISI 1137 Water Quenched & Tempered at 425°C Other notes
A free-cutting version of AISI 1040 grade, used when enhanced machinability is required.

AISI 1137 Water Quenched & Tempered at 425°C Standards with similar compositions

Australia: K1137 to AS 1442
Canada: X46 to CSA B193, X52 to CSA B193
Italy: 35SMn10 to UNI 4838, CF35SMn10 to UNI 4838, CF35SMnPb10 to UNI 4838
Japan: SUM41 to JIS G4804
Mexico: 1132 to NMX-B-301, 1137 to NMX-B-301
Pan America: 1137 to COPANT 330, 1137 to COPANT 331, 1137 to COPANT 332, 1137 to COPANT 514
UK: 36SMn14 to BS EN 10277-3, 36SMnPb14 to BS EN 10277-3
USA: 1132, 1132 to ASTM A29/A29M, 1132 to ASTM A519, 1132 to SAE J403, 1137, 1137 Class A to ASTM A311/A311M, 1137 to ASTM A29/A29M, 1137 to ASTM A519, 1137 to FED QQ-S-633A, 1137 to SAE J403, 5024 to AMS 5024F, G11320 to ASTM A510/A510M, G11320 to ASTM A576-90b, G11370 to ASTM A510/A510M, G11370 to ASTM A576-90b, MIL-S-16124 to MIL-S-16124, UNS G11320, UNS G11370, UNS G11374
Tradenames: A-210.G, 35MNS6, AMERCUT C-1132, AMERCUT C-1137, DUNELT 41, JALCASE 7, S-1137, SAARSTAHL SAE 1137, TRITEX NO. 1