AISI 1025 Normalized Material Data Sheet

AISI 1025 Normalized Material Data Sheet

AISI 1025 Normalized Overview

AISI 1025 normalized is AISI 1025 low carbon steel (UNS G10250) in the normalized condition. This AISI 1025 normalized material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for AISI 1025 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1025 steel parts in-house and inspects them before shipment.

AISI 1025 Normalized Designation

AISI 1025
ConditionNormalized
UNS numberG10250
US nameASME 1025, ASTM M1025, ASTM 1025, ASME G10250, SAE 850, AMS 5045, ~SAE 853 Class 1 Type 5, ~SAE 853 Class 1 Type 4, ~SAE 853 Class 1 Type 3, ~SAE 853 Class 1 Type 2, ~SAE 853 Class 1 Type 1, ~SAE 040S, ~SAE 040C, ~SAE 040B, ~SAE 040A, ~ASTM FPA
EN nameS270GP
EN number1.0023
GB (Chinese) name~ML25Mn
JIS (Japanese) nameSWH 400L, SWH 400, STW 400, STW 370, STPY 400, STKR 400, STKN400W, STK400, SSC 400, SKY 400, SKK 400, SDP2G, SDP2, SDP1TG, SDP1T, ~STPL 380, ~STPG 370, ~STKM13C, ~STKM13B, ~STKM13A, ~STC 590 A, ~STC 510 A, ~STC 440, ~STC 370, ~SPHT 3, ~SM400A

AISI 1025 Normalized Typical uses

General engineering, structural and mechanical engineering.

AISI 1025 Normalized Composition detail

C (carbon)0.22–0.28%
Fe (iron)99–99.5%
Mn (manganese)0.3–0.6%
P (phosphorus)0–0.04%
S (sulfur)0–0.05%

AISI 1025 Normalized Physical properties

Density7.82–7.9g/cm3

AISI 1025 Normalized Mechanical properties

Young’s modulus200–210GPa
Specific stiffness25.4–26.8MN.m/kg
Yield strength (elastic limit)248–274MPa
Tensile strength379–419MPa
Specific strength31.5–34.9kN.m/kg
Elongation25–40% strain
Compressive strength248–274MPa
Flexural modulus200–210GPa
Flexural strength (modulus of rupture)248–274MPa
Shear modulus76–79.9GPa
Bulk modulus185–195GPa
Poisson’s ratio0.32–0.333 
Shape factor62
Hardness – Vickers108–173HV
Elastic stored energy (springs)150–183kJ/m3
Fatigue strength at 10^7 cycles203–293MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
197–303MPa

AISI 1025 Normalized Impact & fracture properties

Fracture toughness41–82MPa.m0.5
Toughness (G)8.96–30kJ/m2

AISI 1025 Normalized Thermal properties

Melting point1480–1530°C
Maximum service temperature432–482°C
Minimum service temperature-68–-38°C
Thermal conductivity51.9–56.2W/m.°C
Specific heat capacity486–506J/kg.°C
Thermal expansion coefficient11.3–11.9µstrain/°C
Thermal shock resistance103–116°C
Thermal distortion resistance4.43–4.87MW/m
Latent heat of fusion270–275kJ/kg

AISI 1025 Normalized Electrical properties

Electrical resistivity15–20µohm.cm
Electrical conductivity8.62–11.5%IACS
Galvanic potential-0.51–-0.43V

AISI 1025 Normalized Magnetic properties

Magnetic typeMagnetic

AISI 1025 Normalized Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5040–5170m/s
Mechanical loss coefficient (tan delta)0.0011–0.0014 

AISI 1025 Normalized Processing properties

Metal castingUnsuitable
Metal cold formingAcceptable
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed39.6 m/min
Weldability
Notes: Preheating and post weld heat treatments may be required
Good
Carbon equivalency0.27 – 0.38

AISI 1025 Normalized Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)
Notes: Aluminum bronze is the most suitable mating material to minimize galling.
Acceptable
FlammabilityNon-flammable

AISI 1025 Normalized Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; Other susceptible environments: Nitrate, hydroxide, carbonate, ammonia
Not susceptible

AISI 1025 Normalized Notes

AISI 1025 Normalized Warning
Some rare heat treatments of certain alloys may produce values for mechanical properties outside the given ranges.

AISI 1025 Normalized Standards with similar compositions

China: ML25 to GB/T 6478
India: 25C4 to IS 11169/1, 25C4 to IS 1570/2/1, C25 to IS 1570/2/1, CEW-2 to IS 3074, ERW-2 to IS 3074, Grade 10 to IS 7887, Grade 10 to IS 8952, Grade 9 to IS 7887, Grade 9 to IS 8952
Japan: SGD 4 to JIS G3108, SWRM 22 to JIS G3505
Mexico: 1023 to NMX-B-301, 1025 to NMX-B-201, 1025 to NMX-B-203-SCFI, 1025 to NMX-B-301
Pan America: 1023 to COPANT 333, 1025 to COPANT 330, 1025 to COPANT 331, 1025 to COPANT 333
South Korea: SGD 4 to KS D 3526, SWRM 22 to KS D 3554
UK: HS22 to BS 1449 Section 1.14
USA: 1023, 1023 to ASTM A29/A29M, 1023 to SAE J403, 1025, 1025 to ASTM A29/A29M, 1025 to ASTM A512-96, 1025 to ASTM A513, 1025 to ASTM A519, 1025 to ASTM A568/A568M, 1025 to MIL-S-11310E, 1025 to MIL-S-7952A, 1025 to MIL-T-3520, 1025 to SAE J403, A to MIL-T-20157, B to MIL-T-20157, C to MIL-T-20157, D to MIL-T-20157, G10230 to ASTM A510/A510M, G10230 to ASTM A576-90b, G10230 to ASTM A830/A830M, G10250 to ASTM A510/A510M, G10250 to ASTM A576-90b, G10250 to ASTM A830/A830M, G10250 to FED QQ-S-700D, M1023, M1023 to ASTM A29/A29M, M1023 to ASTM A575-96, M1023 to SAE J403, M1025, M1025 to ASTM A29/A29M, M1025 to ASTM A575-96, M1025 to SAE J403, UNS G10230, UNS G10230 to UNS, UNS G10250, UNS G10250 to UNS, UNS K02706
Tradenames: GREDE 32, HECLA 35, WITTEN W 25 E