Home » PA (Polyamide / Nylon) » PPA (Polyphthalamide) » PPA Glass Filled Grades » PPA 33% Glass Fiber Flame Retarded Material Data Sheet
PPA 33% Glass Fiber Flame Retarded (Polyphthalamide) Material Data Sheet
PPA 33% Glass Fiber Flame Retarded Overview
PPA 33% glass fiber flame retarded is a grade of polyphthalamide (PPA), designated Polyphthalamide (33% glass fiber, V-0). This PPA 33% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.
PPA 33% Glass Fiber Flame Retarded Designation
Polyphthalamide (33% glass fiber, V-0) Tradenames Amodel, Edgetek, Grivory, Zytel
PPA 33% Glass Fiber Flame Retarded Typical uses
Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications
PPA 33% Glass Fiber Flame Retarded Composition detail
Polymer 52 – 62 % Flame retardant 5 – 15 % Glass (fiber) 33 %
PPA 33% Glass Fiber Flame Retarded Physical properties
PPA 33% Glass Fiber Flame Retarded Mechanical properties
Young’s modulus 11.3 – 14.2 GPa Specific stiffness 6.76 – 8.51 MN.m/kg Yield strength (elastic limit) 131 – 164 MPa Tensile strength 133 – 162 MPa Specific strength 78.4 – 98.3 kN.m/kg Elongation 1.23 – 1.77 % strain Elongation at yield 1.04 – 1.97 % strain Compressive modulus 12.1 – 13.4 GPa Compressive strength 168 – 186 MPa Flexural modulus 12.1 – 14.5 GPa Flexural strength (modulus of rupture) 206 – 252 MPa Shear modulus 4.6 – 4.84 GPa Shear strength 55.8 – 68.2 MPa Bulk modulus 13.5 – 15 GPa Poisson’s ratio 0.337 – 0.351 Shape factor 7.43 Hardness – Vickers 42 – 47 HV Hardness – Rockwell M 175 – 193 Hardness – Rockwell R 175 – 193 Hardness – Shore D 96 – 100 Elastic stored energy (springs) 669 – 1070 kJ/m3 Fatigue strength at 10^7 cycles 56.1 – 62 MPa
PPA 33% Glass Fiber Flame Retarded Impact & fracture properties
Fracture toughness 5.12 – 5.65 MPa.m0.5 Toughness (G) 1.97 – 2.64 kJ/m2 Impact strength, notched 23 °C 8.84 – 17.2 kJ/m2 Impact strength, notched -30 °C 8.19 – 17.8 kJ/m2 Impact strength, unnotched 23 °C 26.3 – 38.7 kJ/m2 Impact strength, unnotched -30 °C 28 – 42 kJ/m2
PPA 33% Glass Fiber Flame Retarded Thermal properties
Melting point 299 – 322 °C Glass temperature 119 – 135 °C Heat deflection temperature 0.45MPa 272 – 327 °C Heat deflection temperature 1.8MPa 247 – 300 °C Maximum service temperature 209 – 228 °C Minimum service temperature -49 – -29 °C Thermal conductivity 0.561 – 0.584 W/m.°C Specific heat capacity 1200 – 1250 J/kg.°C Thermal expansion coefficient 23 – 58 µstrain/°C Thermal shock resistance 197 – 511 °C Thermal distortion resistance 0.00987 – 0.0249 MW/m
PPA 33% Glass Fiber Flame Retarded Electrical properties
Electrical resistivity 2e18 – 5e19 µohm.cm Electrical conductivity 3.45e-18 – 8.62e-17 %IACS Dielectric constant (relative permittivity) 2.24 – 3.16 Dissipation factor (dielectric loss tangent) 0.0033 – 0.0087 Dielectric strength (dielectric breakdown) 22.9 – 39.1 MV/m Comparative tracking index 400 V
PPA 33% Glass Fiber Flame Retarded Magnetic properties
Magnetic type Non-magnetic
PPA 33% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2600 – 2920 m/s Mechanical loss coefficient (tan delta) 0.00689 – 0.00762
PPA 33% Glass Fiber Flame Retarded Absorption & permeability
Water absorption @ 24 hrs 0.15 – 0.25 % Water absorption @ sat 2.9 – 3.9 % Humidity absorption @ sat 1.2 – 1.6 %
PPA 33% Glass Fiber Flame Retarded Processing properties
Polymer injection molding Acceptable Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.4 % Melt temperature 268 – 349 °C Molding pressure range 34.4 – 103 MPa
PPA 33% Glass Fiber Flame Retarded Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing