PPA 15% Glass Fiber Material Data Sheet

PPA 15% Glass Fiber (Polyphthalamide) Material Data Sheet

PPA 15% Glass Fiber Overview

PPA 15% glass fiber is a grade of polyphthalamide (PPA), designated Polyphthalamide (15% glass fiber). This PPA 15% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.

PPA 15% Glass Fiber Designation

Polyphthalamide (15% glass fiber)
TradenamesArlen, Grivory, Tecomid, Zytel

PPA 15% Glass Fiber Typical uses

Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications

PPA 15% Glass Fiber Composition detail

Polymer85  %
Glass (fiber)15  %

PPA 15% Glass Fiber Physical properties

Density1.3–1.33g/cm3

PPA 15% Glass Fiber Mechanical properties

Young’s modulus7.15–8.92GPa
Specific stiffness5.43–6.79MN.m/kg
Yield strength (elastic limit)82.1–102MPa
Tensile strength99.7–122MPa
Specific strength62.4–77.6kN.m/kg
Elongation1.11–1.59% strain
Elongation at yield0.931–1.77% strain
Compressive modulus7.63–8.44GPa
Compressive strength126–140MPa
Flexural modulus6.78–8.12GPa
Flexural strength (modulus of rupture)125–152MPa
Shear modulus2.85–3GPa
Shear strength59.8–73.1MPa
Bulk modulus9.94–11GPa
Poisson’s ratio0.357–0.372 
Shape factor7.5
Hardness – Vickers26–29HV
Hardness – Rockwell M152–168 
Hardness – Rockwell R152–168 
Hardness – Shore D91–95 
Elastic stored energy (springs)417–659kJ/m3
Fatigue strength at 10^7 cycles42.1–46.5MPa

PPA 15% Glass Fiber Impact & fracture properties

Fracture toughness4.66–5.15MPa.m0.5
Toughness (G)2.6–3.47kJ/m2
Impact strength, notched 23 °C17–33kJ/m2
Impact strength, notched -30 °C5.29–11.5kJ/m2
Impact strength, unnotched 23 °C130–190kJ/m2
Impact strength, unnotched -30 °C130–194kJ/m2

PPA 15% Glass Fiber Thermal properties

Melting point299–322°C
Glass temperature119–135°C
Heat deflection temperature 0.45MPa276–332°C
Heat deflection temperature 1.8MPa251–305°C
Maximum service temperature211–230°C
Minimum service temperature-49–-29°C
Thermal conductivity0.399–0.415W/m.°C
Specific heat capacity1480–1540J/kg.°C
Thermal expansion coefficient33–61µstrain/°C
Thermal shock resistance183–356°C
Thermal distortion resistance0.00667–0.0123MW/m

PPA 15% Glass Fiber Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)3.93–5.54 
Dissipation factor (dielectric loss tangent)0.00529–0.0139 
Dielectric strength (dielectric breakdown)17.4–29.6MV/m
Comparative tracking index525–575V

PPA 15% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PPA 15% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2330–2610m/s
Mechanical loss coefficient (tan delta)0.00921–0.0102 

PPA 15% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.19–0.31%
Water absorption @ sat7–9.3%
Humidity absorption @ sat1.9–2.6%

PPA 15% Glass Fiber Processing properties

Polymer injection moldingAcceptable
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.6 – 0.7 %
Melt temperature263 – 338 °C
Molding pressure range34.4 – 103 MPa

PPA 15% Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning