PA66 Lubricated 5% MoS2 (Polyamide 66) Material Data Sheet
PA66 Lubricated 5% MoS2 Overview
PA66 lubricated 5% MoS2 is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, MoS2 Lubricated, Anti-friction). This PA66 lubricated 5% MoS2 material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 Lubricated 5% MoS2 Designation
Polyamide (Nylon) (Type 66, MoS2 Lubricated, Anti-friction) Tradenames Alcom, Ashlene, Bestnyl, Chemlon, Clariant, Delta, Eplamid, Hifill, Hylon, Hyundai, Latilub, LNP Lubricomp, LNP Lubriloy, Lubemid, Lubricomp, Lubrione, Luvocom, Nilamid, Nymax, Nypol, Oxnilon, Plaslube, Plustek, Polynil, Pryme, Radici, Spartech, Terez, Torzen, Tribocomp, Trimid, Vydyne, Zytel
PA66 Lubricated 5% MoS2 Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 Lubricated 5% MoS2 Composition detail
Polymer 95 – 96 % MoS2 (molybdenum disulfide) 4 – 5 %
PA66 Lubricated 5% MoS2 Physical properties
PA66 Lubricated 5% MoS2 Mechanical properties
Young’s modulus 1.54 – 1.91 GPa Specific stiffness 1.32 – 1.64 MN.m/kg Yield strength (elastic limit) 49 – 61.1 MPa Tensile strength 53.4 – 65.3 MPa Specific strength 42 – 52.5 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 19 – 36 % strain Compressive modulus 1.64 – 1.81 GPa Compressive strength 67.7 – 74.8 MPa Flexural modulus 1.59 – 1.91 GPa Flexural strength (modulus of rupture) 60.1 – 73.4 MPa Shear modulus 0.601 – 0.631 GPa Shear strength 32.1 – 39.2 MPa Bulk modulus 2.73 – 3.02 GPa Poisson’s ratio 0.384 – 0.4 Shape factor 4.2 Hardness – Vickers 16 – 17 HV Hardness – Rockwell M 110 – 122 Hardness – Rockwell R 110 – 122 Hardness – Shore D 80 – 83 Elastic stored energy (springs) 693 – 1100 kJ/m3 Fatigue strength at 10^7 cycles 22.6 – 24.9 MPa
PA66 Lubricated 5% MoS2 Impact & fracture properties
Fracture toughness 3.42 – 3.77 MPa.m0.5 Toughness (G) 6.53 – 8.66 kJ/m2 Impact strength, notched 23 °C 4.3 – 5 kJ/m2 Impact strength, notched -30 °C 3.3 – 7.18 kJ/m2 Impact strength, unnotched 23 °C 50 – 107 kJ/m2
PA66 Lubricated 5% MoS2 Thermal properties
Melting point 249 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 202 – 221 °C Heat deflection temperature 1.8MPa 88 – 127 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.282 – 0.293 W/m.°C Specific heat capacity 1570 – 1630 J/kg.°C Thermal expansion coefficient 111 – 116 µstrain/°C Thermal shock resistance 242 – 327 °C Thermal distortion resistance 0.00247 – 0.00261 MW/m
PA66 Lubricated 5% MoS2 Electrical properties
Electrical resistivity 2e17 – 5e18 µohm.cm Electrical conductivity 3.45e-17 – 8.62e-16 %IACS Dielectric constant (relative permittivity) 6.14 – 8.66 Dissipation factor (dielectric loss tangent) 0.0715 – 0.189 Dielectric strength (dielectric breakdown) 12.6 – 21.4 MV/m Comparative tracking index 600 V
PA66 Lubricated 5% MoS2 Magnetic properties
Magnetic type Non-magnetic
PA66 Lubricated 5% MoS2 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1150 – 1280 m/s Mechanical loss coefficient (tan delta) 0.019 – 0.021
PA66 Lubricated 5% MoS2 Absorption & permeability
Water absorption @ 24 hrs 0.6 – 0.98 % Water absorption @ sat 6.7 – 8.9 % Humidity absorption @ sat 2 – 2.6 %
PA66 Lubricated 5% MoS2 Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.7 – 1.8 % Melt temperature 220 – 316 °C Mold temperature 50 – 80 °C Molding pressure range 34.4 – 172 MPa
PA66 Lubricated 5% MoS2 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning