Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Unfilled Grades » PA66 Lubricated 10% PTFE Material Data Sheet
PA66 Lubricated 10% PTFE (Polyamide 66) Material Data Sheet
PA66 Lubricated 10% PTFE Overview
PA66 lubricated 10% PTFE is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, Lubricated, 10% PTFE). This PA66 lubricated 10% PTFE material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 Lubricated 10% PTFE Designation
Polyamide (Nylon) (Type 66, Lubricated, 10% PTFE) Tradenames Alcom, Ashlene, Bestnyl, Chemlon, Clariant, Delta, Eplamid, Hifill, Hylon, Hyundai, Latilub, LNP Lubricomp, LNP Lubriloy, Lubemid, Lubricomp, Lubrione, Luvocom, Nilamid, Nymax, Nypol, Oxnilon, Plaslube, Plustek, Polynil, Pryme, Radici, Spartech, Terez, Torzen, Tribocomp, Trimid, Vydyne, Zytel
PA66 Lubricated 10% PTFE Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 Lubricated 10% PTFE Composition detail
Polymer 90 % PTFE (lubricant) 10 %
PA66 Lubricated 10% PTFE Physical properties
PA66 Lubricated 10% PTFE Mechanical properties
Young’s modulus 1.17 – 1.46 GPa Specific stiffness 0.983 – 1.23 MN.m/kg Yield strength (elastic limit) 35.6 – 44.4 MPa Tensile strength 43.2 – 52.8 MPa Specific strength 29.9 – 37.3 kN.m/kg Elongation 25.3 – 36.3 % strain Elongation at yield 11.7 – 22.2 % strain Compressive modulus 1.25 – 1.38 GPa Compressive strength 54.7 – 60.4 MPa Flexural modulus 1.26 – 1.51 GPa Flexural strength (modulus of rupture) 45 – 55.1 MPa Shear modulus 0.458 – 0.481 GPa Shear strength 25.9 – 31.7 MPa Bulk modulus 2.13 – 2.35 GPa Poisson’s ratio 0.386 – 0.402 Shape factor 4.3 Hardness – Vickers 11 – 13 HV Hardness – Rockwell M 98 – 108 Hardness – Rockwell R 98 – 108 Hardness – Shore D 76 – 79 Elastic stored energy (springs) 479 – 763 kJ/m3 Fatigue strength at 10^7 cycles 18.2 – 20.1 MPa
PA66 Lubricated 10% PTFE Impact & fracture properties
Fracture toughness 3.23 – 3.57 MPa.m0.5 Toughness (G) 7.63 – 10.2 kJ/m2 Impact strength, notched 23 °C 6.4 – 7 kJ/m2 Impact strength, notched -30 °C 3.3 – 7.18 kJ/m2 Impact strength, unnotched 23 °C 55 – 74.7 kJ/m2
PA66 Lubricated 10% PTFE Thermal properties
Melting point 260 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 96 – 133 °C Heat deflection temperature 1.8MPa 71 – 106 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.281 – 0.292 W/m.°C Specific heat capacity 1530 – 1600 J/kg.°C Thermal expansion coefficient 79.4 – 82.6 µstrain/°C Thermal shock resistance 322 – 438 °C Thermal distortion resistance 0.00344 – 0.00363 MW/m
PA66 Lubricated 10% PTFE Electrical properties
Electrical resistivity 5.37e19 – 1.34e21 µohm.cm Electrical conductivity 1.29e-19 – 3.21e-18 %IACS Dielectric constant (relative permittivity) 5.55 – 7.82 Dissipation factor (dielectric loss tangent) 0.0684 – 0.18 Dielectric strength (dielectric breakdown) 32.3 – 55 MV/m Comparative tracking index 600 V
PA66 Lubricated 10% PTFE Magnetic properties
Magnetic type Non-magnetic
PA66 Lubricated 10% PTFE Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 990 – 1110 m/s Mechanical loss coefficient (tan delta) 0.0213 – 0.0236
PA66 Lubricated 10% PTFE Absorption & permeability
Water absorption @ 24 hrs 0.55 – 0.9 % Water absorption @ sat 6.3 – 8.4 % Humidity absorption @ sat 1.8 – 2.5 %
PA66 Lubricated 10% PTFE Processing properties
Polymer injection molding Limited use Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.91 – 1.1 % Melt temperature 223 – 299 °C Mold temperature 70 – 100 °C Molding pressure range 6.88 – 103 MPa
PA66 Lubricated 10% PTFE Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning
Modulus Metal Services