PEK 20-30% Carbon Fiber Material Data Sheet

PEK 20-30% Carbon Fiber (Polyetherketone) Material Data Sheet

PEK 20-30% Carbon Fiber Overview

PEK 20-30% carbon fiber is a grade of polyetherketone (PEK), designated Polyetherketone (20-30% Carbon Fiber). This PEK 20-30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.

PEK Designation

Polyetherketone (20-30% Carbon Fiber)
TradenamesLuvocom; PEEK-HT; Ultrapek

PEK Typical uses

Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.

PEK 20-30% Carbon Fiber Composition detail

Polymer70–80%
Carbon (fiber)20–30%

PEK Physical properties

Density1.4–1.44g/cm3

PEK 20-30% Carbon Fiber Mechanical properties

Young’s modulus19.5–26GPa
Specific stiffness13.7–18.3MN.m/kg
Yield strength (elastic limit)192–208MPa
Tensile strength240–260MPa
Specific strength135–147kN.m/kg
Elongation1.3–1.6% strain
Compressive modulus19.5–26GPa
Compressive strength230–250MPa
Flexural modulus19.5–26GPa
Flexural strength (modulus of rupture)336–360MPa
Shear modulus7.38–9.84GPa
Bulk modulus20.5–21.5GPa
Poisson’s ratio0.315–0.328 
Shape factor8.9
Hardness – Vickers58–62HV
Hardness – Rockwell M100–110 
Hardness – Rockwell R121–133 
Elastic stored energy (springs)755–1040kJ/m3
Fatigue strength at 10^7 cycles87.7–114MPa

PEK Impact & fracture properties

Fracture toughness6.72–8.81MPa.m0.5
Toughness (G)1.98–3.5kJ/m2
Impact strength, notched 23 °C8.18–9.9kJ/m2
Impact strength, notched -30 °C7.27–8.8kJ/m2
Impact strength, unnotched 23 °C50–60.5kJ/m2
Impact strength, unnotched -30 °C50–60.5kJ/m2

PEK 20-30% Carbon Fiber Thermal properties

Melting point368–394°C
Glass temperature182–200°C
Heat deflection temperature 0.45MPa310–350°C
Heat deflection temperature 1.8MPa225–276°C
Vicat softening point310–350°C
Maximum service temperature226–246°C
Minimum service temperature-47–-27°C
Thermal conductivity0.653–0.679W/m.°C
Specific heat capacity1360–1420J/kg.°C
Thermal expansion coefficient18–36µstrain/°C
Thermal shock resistance241–503°C
Thermal distortion resistance0.0185–0.037MW/m

PEK Electrical properties

Electrical resistivity30000000–160000000µohm.cm
Electrical conductivity1.08e-6–5.75e-6%IACS
Galvanic potential0.14–0.22V

PEK Magnetic properties

Magnetic typeNon-magnetic

PEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3700–4290m/s
Mechanical loss coefficient (tan delta)0.00409–0.005 

PEK Absorption & permeability

Water absorption @ 24 hrs0.1–0.2%

PEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Linear mold shrinkage0.1 – 2 %
Melt temperature344 – 430 °C
Molding pressure range68.8 – 138 MPa

PEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing