Home » PEK (Polyetherketone) » PEK 30% Glass Fiber Material Data Sheet
PEK 30% Glass Fiber (Polyetherketone) Material Data Sheet
PEK 30% Glass Fiber Overview
PEK 30% glass fiber is a grade of polyetherketone (PEK), designated Polyetherketone (30% Glass Fiber). This PEK 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEK parts in-house and inspects them before shipment.
PEK Designation
Polyetherketone (30% Glass Fiber) Tradenames Arylmax, Avaspire, G-Paek, Victrex
PEK Typical uses
Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, housing for tire pressure sensors, valve spring discs, rollers, guides, gears, reciprocating components.
PEK 30% Glass Fiber Composition detail
Polymer 70 % Glass (fiber) 30 %
PEK Physical properties
PEK 30% Glass Fiber Mechanical properties
Young’s modulus 9.72 – 12.1 GPa Specific stiffness 6.47 – 8.08 MN.m/kg Yield strength (elastic limit) 130 – 152 MPa Tensile strength 163 – 190 MPa Specific strength 86.7 – 102 kN.m/kg Elongation 2.2 – 3.4 % strain Compressive modulus 9.72 – 12.1 GPa Compressive strength 197 – 217 MPa Flexural modulus 10.7 – 11.3 GPa Flexural strength (modulus of rupture) 235 – 250 MPa Shear modulus 3.6 – 4.48 GPa Bulk modulus 11.8 – 12.4 GPa Poisson’s ratio 0.344 – 0.358 Shape factor 6.9 Hardness – Vickers 39 – 46 HV Hardness – Rockwell M 97 – 107 Hardness – Rockwell R 120 – 132 Elastic stored energy (springs) 763 – 1090 kJ/m3 Fatigue strength at 10^7 cycles 76 – 84 MPa
PEK Impact & fracture properties
Fracture toughness 4.94 – 7.55 MPa.m0.5 Toughness (G) 2.31 – 5.11 kJ/m2 Impact strength, notched 23 °C 9.09 – 11 kJ/m2 Impact strength, notched -30 °C 8.18 – 9.9 kJ/m2 Impact strength, unnotched 23 °C 63.6 – 77 kJ/m2 Impact strength, unnotched -30 °C 68.2 – 82.5 kJ/m2
PEK 30% Glass Fiber Thermal properties
Melting point 329 – 381 °C Glass temperature 182 – 200 °C Heat deflection temperature 0.45MPa 340 – 350 °C Heat deflection temperature 1.8MPa 326 – 350 °C Vicat softening point 340 – 350 °C Maximum service temperature 235 – 255 °C Minimum service temperature -47 – -27 °C Thermal conductivity 0.494 – 0.513 W/m.°C Specific heat capacity 1310 – 1370 J/kg.°C Thermal expansion coefficient 33.3 – 36 µstrain/°C Thermal shock resistance 327 – 430 °C Thermal distortion resistance 0.0139 – 0.0152 MW/m
PEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.14 – 3.46 Dissipation factor (dielectric loss tangent) 0.00398 – 0.00477 Dielectric strength (dielectric breakdown) 14 – 15.1 MV/m Comparative tracking index 175 – 225 V
PEK Magnetic properties
Magnetic type Non-magnetic
PEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2540 – 2850 m/s Mechanical loss coefficient (tan delta) 0.00698 – 0.00814
PEK Absorption & permeability
Water absorption @ 24 hrs 0.06 – 0.08 %
PEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.1 – 0.9 % Melt temperature 334 – 429 °C Molding pressure range 68.8 – 138 MPa
PEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Good Flammability Self-extinguishing
PEK Notes
PEK 30% Glass Fiber Other notes Endurance limit tested at 15 Hz
Modulus Metal Services