Modified PEEK 45-55% Carbon High Load Material Data Sheet

Modified PEEK 45-55% Carbon High Load (Polyetheretherketone) Material Data Sheet

Modified PEEK 45-55% Carbon High Load Overview

Modified PEEK 45-55% carbon high load is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (Wear grade). This modified PEEK 45-55% carbon high load material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

Modified PEEK Designation

Modified poly(etheretherketone) (Wear grade)
TradenamesAvaSpire

Modified PEEK 45-55% Carbon High Load Composition detail

Polymer45–55%
PTFE (lubricant)0–10%
Carbon (fiber)35–45%
Graphite (powder)0–10%

Modified PEEK Physical properties

Density1.51–1.55g/cm3

Modified PEEK 45-55% Carbon High Load Mechanical properties

Young’s modulus32.8–34.4GPa
Specific stiffness21.4–22.6MN.m/kg
Yield strength (elastic limit)131–144MPa
Tensile strength161–177MPa
Specific strength85.5–94.2kN.m/kg
Elongation0.833–0.968% strain
Elongation at yield0.83–0.97% strain
Compressive modulus32.8–34.4GPa
Flexural modulus32.8–34.4GPa
Flexural strength (modulus of rupture)244–256MPa
Shear modulus12–13GPa
Shear strength66.5–73.5MPa
Poisson’s ratio0.42–0.46 
Shape factor14.6
Hardness – Vickers39–43HV
Elastic stored energy (springs)255–309kJ/m3
Fatigue strength at 10^7 cycles64.2–71MPa

Modified PEEK Impact & fracture properties

Impact strength, notched 23 °C4.77–5.83kJ/m2
Impact strength, unnotched 23 °C28.8–35.2kJ/m2

Modified PEEK 45-55% Carbon High Load Thermal properties

Melting point608–624°C
Glass temperature150–168°C
Heat deflection temperature 0.45MPa558–572°C
Heat deflection temperature 1.8MPa544–558°C
Vicat softening point558–572°C
Thermal conductivity0.686–0.714W/m.°C
Specific heat capacity1290–1320J/kg.°C
Thermal expansion coefficient6.91–7.09µstrain/°C
Thermal shock resistance553–617°C
Thermal distortion resistance0.0976–0.102MW/m

Modified PEEK Electrical properties

Electrical resistivity25000000000000000–100000000000000000µohm.cm
Electrical conductivity1.72e-15–6.9e-15%IACS
Dielectric constant (relative permittivity)3.3–4 
Dissipation factor (dielectric loss tangent)0.001–0.006 
Dielectric strength (dielectric breakdown)30–70MV/m
Galvanic potential0.14–0.22V

Modified PEEK Magnetic properties

Magnetic typeNon-magnetic

Modified PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity4620–4750m/s

Modified PEEK Absorption & permeability

Water absorption @ 24 hrs0.009–0.011%

Modified PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionAcceptable
Polymer thermoformingUnsuitable
Melt temperature366 – 388 °C
Mold temperature149 – 177 °C

Modified PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing