Modified PEEK 30% Carbon Fiber Material Data Sheet

Modified PEEK 30% Carbon Fiber (Polyetheretherketone) Material Data Sheet

Modified PEEK 30% Carbon Fiber Overview

Modified PEEK 30% carbon fiber is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (30% carbon fiber). This modified PEEK 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

Modified PEEK Designation

Modified poly(etheretherketone) (30% carbon fiber)
TradenamesAvaSpire

Modified PEEK 30% Carbon Fiber Composition detail

Polymer70  %
Carbon (fiber)30  %

Modified PEEK Physical properties

Density1.41–1.43g/cm3

Modified PEEK 30% Carbon Fiber Mechanical properties

Young’s modulus17.5–22.4GPa
Specific stiffness12.3–15.8MN.m/kg
Yield strength (elastic limit)145–160MPa
Tensile strength178–199MPa
Specific strength102–113kN.m/kg
Elongation1.33–2.14% strain
Elongation at yield1.3–2.1% strain
Compressive modulus17.5–22.4GPa
Flexural modulus15.1–19.3GPa
Flexural strength (modulus of rupture)260–302MPa
Shear modulus6.5–8.3GPa
Shear strength90–99MPa
Poisson’s ratio0.42–0.46 
Shape factor9.81
Hardness – Vickers43–47HV
Elastic stored energy (springs)502–683kJ/m3
Fatigue strength at 10^7 cycles71.6–79.1MPa

Modified PEEK Impact & fracture properties

Impact strength, notched 23 °C5.23–6.84kJ/m2
Impact strength, unnotched 23 °C53.2–64.2kJ/m2

Modified PEEK 30% Carbon Fiber Thermal properties

Melting point613–618°C
Glass temperature150–168°C
Heat deflection temperature 0.45MPa495–563°C
Heat deflection temperature 1.8MPa483–549°C
Vicat softening point495–563°C
Thermal conductivity0.34–0.36W/m.°C
Specific heat capacity1400–1420J/kg.°C
Thermal expansion coefficient5–8.2µstrain/°C
Thermal shock resistance913–1580°C
Thermal distortion resistance0.0426–0.0701MW/m

Modified PEEK Electrical properties

Electrical resistivity10–100µohm.cm
Electrical conductivity1.72–17.2%IACS
Dielectric constant (relative permittivity)3.3–4 
Dielectric strength (dielectric breakdown)30–70MV/m
Galvanic potential0.14–0.22V

Modified PEEK Magnetic properties

Magnetic typeNon-magnetic

Modified PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3500–3980m/s

Modified PEEK Processing properties

Polymer injection moldingUnsuitable
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Melt temperature366 – 388 °C
Mold temperature149 – 204 °C

Modified PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing