Home » PEEK (Polyetheretherketone) » PEEK 30% Carbon Fiber Lubricated Material Data Sheet
PEEK 30% Carbon Fiber Lubricated (Polyetheretherketone) Material Data Sheet
PEEK 30% Carbon Fiber Lubricated Overview
PEEK 30% carbon fiber lubricated is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (30% Carbon Fiber, Lubricated). This PEEK 30% carbon fiber lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (30% Carbon Fiber, Lubricated) Tradenames Inlube, Latilub, RTP, Witcom
PEEK Typical uses
Aerospace applications, automotive applications, high temperature applications
PEEK 30% Carbon Fiber Lubricated Composition detail
Polymer 55 – 65 % PTFE (lubricant) 5 – 15 % Carbon (fiber) 30 %
PEEK Physical properties
PEEK 30% Carbon Fiber Lubricated Mechanical properties
Young’s modulus 22 – 27.6 GPa Specific stiffness 14.8 – 18.6 MN.m/kg Yield strength (elastic limit) 159 – 228 MPa Tensile strength 190 – 230 MPa Specific strength 107 – 154 kN.m/kg Elongation 1 – 1.3 % strain Elongation at yield 1 – 2 % strain Compressive modulus 14.4 – 15.1 GPa Compressive strength 239 – 264 MPa Flexural modulus 18.5 – 25.5 GPa Flexural strength (modulus of rupture) 255 – 345 MPa Shear modulus 8.34 – 8.76 GPa Shear strength 120 – 132 MPa Bulk modulus 22 – 27.6 GPa Poisson’s ratio 0.43 – 0.45 Shape factor 9.8 Hardness – Vickers 47 – 51 HV Hardness – Rockwell R 124 – 125 Hardness – Shore D 97 – 105 Elastic stored energy (springs) 521 – 1040 kJ/m3 Fatigue strength at 10^7 cycles 76.1 – 92 MPa
PEEK Impact & fracture properties
Fracture toughness 6.56 – 9.44 MPa.m0.5 Toughness (G) 1.78 – 3.57 kJ/m2 Impact strength, notched 23 °C 6.52 – 9.6 kJ/m2 Impact strength, unnotched 23 °C 43 – 75 kJ/m2
PEEK 30% Carbon Fiber Lubricated Thermal properties
Melting point 343 °C Glass temperature 321 – 334 °C Heat deflection temperature 0.45MPa 295 – 350 °C Heat deflection temperature 1.8MPa 288 – 323 °C Vicat softening point 350 °C Maximum service temperature 260 – 280 °C Thermal conductivity 0.87 – 0.97 W/m.°C Specific heat capacity 1320 – 1380 J/kg.°C Thermal expansion coefficient 14 – 15 µstrain/°C Thermal shock resistance 432 – 659 °C Thermal distortion resistance 0.0595 – 0.0676 MW/m
PEEK Electrical properties
Electrical resistivity 5500000000 – 65800000000 µohm.cm Electrical conductivity 2.62e-9 – 3.13e-8 %IACS Dielectric constant (relative permittivity) 3.2 – 3.4 Galvanic potential 0.14 – 0.22 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3840 – 4320 m/s Mechanical loss coefficient (tan delta) 0.0044 – 0.0064
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.1 – 0.12 % Water absorption @ sat 0.3 % Humidity absorption @ sat 0.1 %
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.05 – 0.19 % Melt temperature 349 – 410 °C Mold temperature 154 – 218 °C Molding pressure range 68.9 – 124 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing