Home » PEEK (Polyetheretherketone) » PEEK 40% Carbon Fiber Material Data Sheet
PEEK 40% Carbon Fiber (Polyetheretherketone) Material Data Sheet
PEEK 40% Carbon Fiber Overview
PEEK 40% carbon fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (40% Carbon Fiber). This PEEK 40% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (40% Carbon Fiber) Tradenames Edgetek, Hifill, Larpeek, LNP Thermocomp, Luvocom, RTP, Victrex
PEEK Typical uses
Aerospace applications, automotive applications, bearings, bushings, gears, general purpose, medical/healthcare applications, metal replacement, parts (engineering), pump parts, textile applications
PEEK 40% Carbon Fiber Composition detail
Polymer 60 % Carbon (fiber) 40 %
PEEK Physical properties
PEEK 40% Carbon Fiber Mechanical properties
Young’s modulus 33.4 – 40 GPa Specific stiffness 22.9 – 27.5 MN.m/kg Yield strength (elastic limit) 241 – 269 MPa Tensile strength 241 – 316 MPa Specific strength 165 – 185 kN.m/kg Elongation 1 – 1.5 % strain Elongation at yield 1.3 – 1.4 % strain Compressive modulus 21.4 – 22.5 GPa Compressive strength 225 – 301 MPa Flexural modulus 27.1 – 34 GPa Flexural strength (modulus of rupture) 352 – 470 MPa Shear modulus 12.1 – 12.7 GPa Shear strength 126 MPa Bulk modulus 33.4 – 40 GPa Poisson’s ratio 0.47 Shape factor 10.5 Hardness – Vickers 62 – 67 HV Hardness – Rockwell R 118 Hardness – Shore D 88 – 89 Elastic stored energy (springs) 773 – 1020 kJ/m3 Fatigue strength at 10^7 cycles 100 – 121 MPa
PEEK Impact & fracture properties
Fracture toughness 8.32 – 12 MPa.m0.5 Toughness (G) 1.93 – 3.86 kJ/m2 Impact strength, notched 23 °C 5 – 11 kJ/m2 Impact strength, unnotched 23 °C 40 – 86 kJ/m2
PEEK 40% Carbon Fiber Thermal properties
Melting point 343 °C Glass temperature 143 °C Heat deflection temperature 0.45MPa 300 – 339 °C Heat deflection temperature 1.8MPa 288 – 349 °C Vicat softening point 300 °C Maximum service temperature 235 – 250 °C Thermal conductivity 2 W/m.°C Specific heat capacity 1800 J/kg.°C Thermal expansion coefficient 4 – 7.6 µstrain/°C Thermal shock resistance 907 – 1760 °C Thermal distortion resistance 0.263 – 0.5 MW/m
PEEK Electrical properties
Electrical resistivity 100000000000 – 1000000000000 µohm.cm Electrical conductivity 1.72e-10 – 1.72e-9 %IACS Dielectric constant (relative permittivity) 3.2 – 3.4 Dissipation factor (dielectric loss tangent) 0.005 Galvanic potential 0.14 – 0.22 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 4780 – 5250 m/s Mechanical loss coefficient (tan delta) 0.0036 – 0.0053
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.03 – 0.12 % Water absorption @ sat 0.3 % Humidity absorption @ sat 0.3 %
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.05 – 0.5 % Melt temperature 349 – 400 °C Mold temperature 121 – 260 °C Molding pressure range 68.9 – 207 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing