Home » PEEK (Polyetheretherketone) » PEEK 30% Glass Fiber Material Data Sheet
PEEK 30% Glass Fiber (Polyetheretherketone) Material Data Sheet
PEEK 30% Glass Fiber Overview
PEEK 30% glass fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (30% Glass Fiber). This PEEK 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (30% Glass Fiber) Tradenames Dynamix, Edgetek, Gatone, Hifill, Kebapeak, Ketaspire, Ketron, Larpeek, LNP Thermocomp, Luvocom, Pyramid, Schulatec, Vestakeep, Victrex
PEEK Typical uses
Wire covering, injection molded engineering products, film for flexible pcb, resin in fiber prepegs, aerospace applications, radiation environments.
PEEK 30% Glass Fiber Composition detail
Polymer 70 % Glass (fiber) 30 %
PEEK Physical properties
PEEK 30% Glass Fiber Mechanical properties
Young’s modulus 8.62 – 11 GPa Specific stiffness 5.69 – 7.27 MN.m/kg Yield strength (elastic limit) 124 – 158 MPa Tensile strength 155 – 197 MPa Specific strength 81.8 – 104 kN.m/kg Elongation 2 – 3 % strain Compressive modulus 8.62 – 11 GPa Compressive strength 147 – 154 MPa Flexural modulus 8.66 – 11 GPa Flexural strength (modulus of rupture) 228 – 290 MPa Shear modulus 3.18 – 4.06 GPa Bulk modulus 10.9 – 11.5 GPa Poisson’s ratio 0.39 – 0.41 Shape factor 6.5 Hardness – Vickers 37 – 47 HV Hardness – Rockwell M 98 – 108 Hardness – Rockwell R 120 – 132 Elastic stored energy (springs) 780 – 1290 kJ/m3 Fatigue strength at 10^7 cycles 61.7 – 80.3 MPa
PEEK Impact & fracture properties
Fracture toughness 5.34 – 7.93 MPa.m0.5 Toughness (G) 2.98 – 6.33 kJ/m2 Impact strength, notched 23 °C 9.09 – 11 kJ/m2 Impact strength, notched -30 °C 8.18 – 9.9 kJ/m2 Impact strength, unnotched 23 °C 63.6 – 77 kJ/m2 Impact strength, unnotched -30 °C 68.2 – 82.5 kJ/m2
PEEK 30% Glass Fiber Thermal properties
Melting point 322 – 346 °C Glass temperature 143 – 157 °C Heat deflection temperature 0.45MPa 306 – 356 °C Heat deflection temperature 1.8MPa 288 – 315 °C Maximum service temperature 260 – 280 °C Minimum service temperature -70 – -50 °C Thermal conductivity 0.197 – 0.213 W/m.°C Specific heat capacity 1000 – 1100 J/kg.°C Thermal expansion coefficient 20 – 30 µstrain/°C Thermal shock resistance 455 – 755 °C Thermal distortion resistance 0.00681 – 0.0103 MW/m
PEEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.2 – 3.4 Dissipation factor (dielectric loss tangent) 0.0019 – 0.0021 Dielectric strength (dielectric breakdown) 16.5 – 19.8 MV/m Comparative tracking index 175 – 225 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2380 – 2700 m/s Mechanical loss coefficient (tan delta) 0.00747 – 0.00886
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.06 – 0.12 %
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 1.4 % Melt temperature 305 – 399 °C Mold temperature 120 – 160 °C Molding pressure range 68.8 – 138 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
Modulus Metal Services