Home » PEEK (Polyetheretherketone) » PEEK 15% Glass Fiber Material Data Sheet
PEEK 15% Glass Fiber (Polyetheretherketone) Material Data Sheet
PEEK 15% Glass Fiber Overview
PEEK 15% glass fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (15% Glass Fiber). This PEEK 15% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (15% Glass Fiber) Tradenames Ketaspire, Larpeek, LNP Thermocomp, Luvocom, RTP, Vampeek, Victrex
PEEK Typical uses
Aerospace applications, automotive applications, connectors, dental applications, electrical/electronic applications, film, food applications (non-specific), hospital goods, industrial applications, medical appliances, oil/gas applications, parts (engineering), pump parts, seals, surgical instruments, textile applications
PEEK 15% Glass Fiber Composition detail
Polymer 85 % Glass (fiber) 15 %
PEEK Physical properties
PEEK 15% Glass Fiber Mechanical properties
Young’s modulus 6.38 – 7.56 GPa Specific stiffness 4.57 – 5.43 MN.m/kg Yield strength (elastic limit) 110 – 137 MPa Tensile strength 117 – 140 MPa Specific strength 78.8 – 98.3 kN.m/kg Elongation 2.32 – 4.8 % strain Elongation at yield 2 – 3.9 % strain Compressive modulus 4.07 – 4.27 GPa Compressive strength 200 MPa Flexural modulus 5.6 – 7.5 GPa Flexural strength (modulus of rupture) 193 – 240 MPa Shear modulus 2.42 – 2.54 GPa Shear strength 73.1 – 80.6 MPa Bulk modulus 6.38 – 7.56 GPa Poisson’s ratio 0.39 – 0.41 Shape factor 5.7 Hardness – Vickers 30 – 32 HV Hardness – Shore D 86 Elastic stored energy (springs) 869 – 1350 kJ/m3 Fatigue strength at 10^7 cycles 46.5 – 56.3 MPa
PEEK Impact & fracture properties
Fracture toughness 6.39 – 9.2 MPa.m0.5 Toughness (G) 6 – 11.9 kJ/m2 Impact strength, notched 23 °C 4.82 – 9.1 kJ/m2 Impact strength, notched -30 °C 3 kJ/m2 Impact strength, unnotched 23 °C 45 – 91 kJ/m2 Impact strength, unnotched -30 °C 40 kJ/m2
PEEK 15% Glass Fiber Thermal properties
Melting point 343 °C Glass temperature 143 °C Heat deflection temperature 0.45MPa 290 – 329 °C Heat deflection temperature 1.8MPa 216 – 321 °C Vicat softening point 300 – 335 °C Maximum service temperature 220 – 250 °C Thermal conductivity 0.3 W/m.°C Specific heat capacity 1700 J/kg.°C Thermal expansion coefficient 25 – 50 µstrain/°C Thermal shock resistance 347 – 719 °C Thermal distortion resistance 0.006 – 0.012 MW/m
PEEK Electrical properties
Electrical resistivity 1000000000000000000000 – 10000000000000000000000 µohm.cm Electrical conductivity 1.72e-20 – 1.72e-19 %IACS Dielectric constant (relative permittivity) 3.1 Dielectric strength (dielectric breakdown) 23 – 24 MV/m Comparative tracking index 150 – 200 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2140 – 2330 m/s Mechanical loss coefficient (tan delta) 0.0084 – 0.012
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.06 – 0.17 % Humidity absorption @ sat 0.4 %
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.3 – 0.9 % Melt temperature 349 – 400 °C Mold temperature 149 – 218 °C Molding pressure range 68.9 – 124 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
Modulus Metal Services