Home » Gunmetal Alloys » CuSn7Zn2Ni5 Nickel Gunmetal, Cast, Aged Material Data Sheet
CuSn7Zn2Ni5 Nickel Gunmetal, Cast, Aged Material Data Sheet
CuSn7Zn2Ni5 Nickel Gunmetal Material Data Sheet (Cast, Aged)
CuSn7Zn2Ni5 Cast Aged Gunmetal Overview
CuSn7Zn2Ni5 cast aged gunmetal is a cast gunmetal, known as nickel gunmetal. Condition: Aged. This CuSn7Zn2Ni5 cast aged gunmetal material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for CuSn7Zn2Ni5 gunmetal castings from Turkey (Türkiye)? Modulus Metal supplies CuSn7Zn2Ni5 gunmetal castings with in-house CNC machining and inspects them before shipment.
CuSn7Zn2Ni5 Designation
Copper Alloy: CuSn7Zn2Ni5
Condition
Aged
CuSn7Zn2Ni5 Typical uses
Pumps and valves, bearings, valve guides, marine uses, applications in high so2 atmospheres, slow-moving bearings, liners, bearing cages, switch parts, trolley hangers.