Custom 465 H950 Stainless Steel Material Data Sheet
Custom 465 H950 Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
Custom 465 H950 Stainless Steel Overview
Custom 465 H950 stainless steel is a martensitic precipitation hardening stainless steel (UNS S46500) in the wrought form. Condition: H950 (Solution annealed; precipitation (age) hardened at 510°C; air cooled). This Custom 465 H950 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for Custom 465 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined Custom 465 parts in-house and inspects them before shipment.
Custom 465 Designation
Custom 465, wrought
Condition
H950 (Solution annealed; precipitation (age) hardened at 510°C; air cooled)
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide
Susceptible
Intergranular (weld line) corrosion
Good
Inorganic acids
Restricted
Organic acids
Restricted
Alkalis
Moderate
Humidity / water
Excellent
Sea water
Restricted
Sour oil and gas
Good
Custom 465 Notes
Custom 465 H950 Warning
Certain processing procedures may cause these extrusions to become susceptible to stress-corrosion cracking
Custom 465 H950 Other notes
Custom 465® stainless is a double-vacuum melted, martensitic, age-hardenable alloy. This alloy was designed to have excellent notch tensile strength and fracture toughness over a wide range of section sizes. In the H950 condition, the alloy achieves a minimum ultimate tensile strength of 240 ksi while retaining good toughness and resistance to stress-corrosion cracking. Custom 465 stainless provides a superior combination of strength, toughness and stress corrosion cracking resistance compared with other high-strength PH stainless alloys such as Custom 455® stainless or PH13-8Mo® stainless.
Custom 465 Standards with similar compositions
USA: S46500 to ASTM A564/A564M, S46500 to ASTM A693, S46500 to ASTM A959, UNS S46500