PH15-7Mo TH1050 Stainless Steel Material Data Sheet
PH15-7Mo TH1050 Stainless Steel Material Data Sheet (Semi-austenitic, Precipitation Hardened)
PH15-7Mo TH1050 Stainless Steel Overview
PH15-7Mo TH1050 stainless steel is a semi-austenitic precipitation hardening stainless steel (UNS S15700) in the wrought form. Condition: TH1050 (Solution annealed; precipitation (age) hardened at 566°C; air cooled). This PH15-7Mo TH1050 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for PH15-7Mo parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PH15-7Mo parts in-house and inspects them before shipment.
PH15-7Mo Designation
Korloy 2573, wrought
Condition
TH1050 (Solution annealed; precipitation (age) hardened at 566°C; air cooled)
UNS number
S15700
US name
PH15-7Mo
PH15-7Mo Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide
Susceptible
Intergranular (weld line) corrosion
Good
Inorganic acids
Restricted
Organic acids
Restricted
Alkalis
Moderate
Humidity / water
Excellent
Sea water
Restricted
Sour oil and gas
Restricted
PH15-7Mo Notes
PH15-7Mo TH1050 Warning
Check with supplier what tempering and aging procedure has been applied – it could make a major difference to the steel’s mechanical properties.
PH15-7Mo Standards with similar compositions
China: 0Cr15Ni7Mo2Al to GB 1220
France: Z8CNDA15.07 to AFNOR NF A35-581
Germany: 1.4532 to DIN EN 10088, X8CrNiMoAl15-7-2 to DIN EN 10088
USA: 5520 to AMS 5520, 63 to ASTM A579, PH 15-7 Mo to SAE J467, S15700 to ASTM A564/A564M, S15700 to ASTM A693, S15700 to ASTM A705/A705M-95, S15700 to ASTM A959, UNS S14800, UNS S15700, UNS S15780, UNS S15789
Tradenames: AL 15-7, KRUPP WL 1.4574, NIROSTA 4532, WIRONIT 151 L