Custom 455 H950 Stainless Steel Material Data Sheet
Custom 455 H950 Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
Custom 455 H950 Stainless Steel Overview
Custom 455 H950 stainless steel is a martensitic precipitation hardening stainless steel (UNS S45500) in the wrought form. Condition: H950 (Solution annealed; precipitation (age) hardened at 510°C; air cooled). This Custom 455 H950 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for Custom 455 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined Custom 455 parts in-house and inspects them before shipment.
Custom 455 Designation
Custom 455, wrought
Condition
H950 (Solution annealed; precipitation (age) hardened at 510°C; air cooled)
UNS number
S45500
US name
Custom 455
Custom 455 Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes