Base Fe (Iron) : Fe54-62 / Ni34-36 / Cr2-3 / Si1.5-3 / Mn0.5-1.5
Impurities: C<2.4, Cu<0.5, P<0.08
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 2.4 | % |
| Cr | (chromium) | 2 | 3 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 53.5 | 62 | % |
| Mn | (manganese) | 0.5 | 1.5 | % |
| Ni | (nickel) | 34 | 36 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 1.5 | 3 | % |
Common Uses:
Components that are used in low temperature compressors, pressure vessels in air-blast circuit breakers, and pumps.
| Similar-composition standards with EN GJSA XNiCr35 3 |
|---|
| AFNOR NFA32301 SNC353 (France) |
| DIN WNr 0.7685 (Germany) |
| DIN 1694 GGG-NiCr353 (Germany) |
| DIN 1694 GGG-NiSiCr3552 (Germany) |
| ISO 2892(73) S-NiCr353 (International) |
| BS 3468 S-5S (United Kingdom) |
| BS 3468 S-NiCr353 (United Kingdom) |
| ASTM A439(94) D-5B (USA) |
| ASTM A439(94) D-5S (USA) |