Base Fe (Iron) : Fe57-68 / Ni28-32 / Cr2.5-3.5 / Si1.5-3 / Mn0.5-1.5 Impurities: C<2.6, Cu<0.5, P<0.08 Elements Symbol Elements Name Min Max % C (carbon) 0 2.6 % Cr (chromium) 2.5 3.5 % Cu (copper) 0 0.5 % Fe (iron) 56.8 67.5 % Mn (manganese) 0.5 1.5 % Ni (nickel) 28 32 % P (phosphorus) 0 … Continue reading EN GJSA XNiCr30 3 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY