EN GJSA XNiCr20 2 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe66-79 / Ni18-22 / Cr1-3.5 / Si1.5-3 / Mn0.5-1.5 Impurities: C<3, Cu<0.5, P<0.08 Elements Symbol Elements Name Min Max % C (carbon) 0 3 % Cr (chromium) 1 3.5 % Cu (copper) 0 0.5 % Fe (iron) 66.4 79 % Mn (manganese) 0.5 1.5 % Ni (nickel) 18 22 % P (phosphorus) 0 … Continue reading EN GJSA XNiCr20 2 Cast Iron Chemical Composition (austenitic, nodular) | Modulus Metal | Supplier Company | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY