Base Fe (Iron) : Fe67-79 / Ni18-22 / Cr1-3.5 / Si1.5-2.4 / Mn0.5-1.5 / Nb0.12-0.2
Impurities: C<3, Cu<0.5, P<0.08
| Elements Symbol | Elements Name | Min | Max | % |
|---|---|---|---|---|
| C | (carbon) | 0 | 3 | % |
| Cr | (chromium) | 1 | 3.5 | % |
| Cu | (copper) | 0 | 0.5 | % |
| Fe | (iron) | 66.8 | 78.9 | % |
| Mn | (manganese) | 0.5 | 1.5 | % |
| Nb | (niobium) | 0.12 | 0.2 | % |
| Ni | (nickel) | 18 | 22 | % |
| P | (phosphorus) | 0 | 0.08 | % |
| Si | (silicon) | 1.5 | 2.4 | % |
Common Uses:
Equipment such as pumps, valves, compressors, bushings, and turbo-supercharger housings made of exhaust gas manifolds that can function at high temperatures up to 1000 K would benefit from superior weldability in their design and construction. These types of components are often used in applications where strong and reliable welds are important.
| Similar-composition standards with EN GJSA XNiCrNb20 2 |
|---|
| Germany: GGG-NiCrNb202 to DIN 1694 |
| Japan: FCDA-NiCrNb 20 2 to JIS G5510 |
| UK: S-2W to BS 3468 |