EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.0C/1.7Si/1.1Ni/0.6Mn/0.5Cr/<0.2P/<0.12S

EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite)
Material Standards with Similar Chemical Composition
NBN 83001 FGG30 (Belgium)
GB 9439(88) HT 300 (China)
DS 11301 GG30 (Denmark)
AFNOR NFA32101 FGL300 (France)
AFNOR NFA32101 FGL350A (France)
AFNOR NFA32101 FGL400A (France)
DIN WNr 0.6025 (Germany)
DIN 1691 GG25 (Germany)
IS 210 FG300 (India)
UNI 5007 G30 (Italy)
JIS G5501(95) FC300 (Japan)
NEN 6002A GG30 (Netherlands)
NS 722 SjG30 (Norway)
NS 722 SjG350 (Norway)
AS 1830(86) T300 (NSW Australia)
GOST 1412 SCh30 (Russian Federation)
SABS 1034 300 (South Africa)
ISO 185(88) 300 (International)
BS 1452 300 (United Kingdom)
ASME SA278 45 (USA)
ASTM A278(93) 45 (USA)
ASTM A278M(93) 300 (USA)
ASTM A278M(93) 325 (USA)
ASTM A48(94) 45A (USA)
ASTM A48(94) 45B (USA)
ASTM A48(94) 45C (USA)
ASTM A48(94) 45S (USA)