Home » PA (Polyamide / Nylon) » PA11 (Polyamide 11 / Nylon 11) » PA11 Unfilled Grades » PA11 Semi-Flexible Grade Material Data Sheet
PA11 Semi-Flexible Grade (Polyamide 11) Material Data Sheet
PA11 Semi-Flexible Grade Overview
PA11 semi-flexible grade is a grade of polyamide 11 (PA11, nylon 11), designated Polyamide (Nylon) (Type 11, semi-flexible, molding & extrusion). This PA11 semi-flexible grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA11 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA11 parts in-house and inspects them before shipment.
PA11 Semi-Flexible Grade Designation
Polyamide (Nylon) (Type 11, semi-flexible, molding & extrusion) Tradenames Rilsan
PA11 Semi-Flexible Grade Typical uses
Hose for air, hydraulic fluid or petrol, gears, cams, tool handles, powder for coatings for metals.
PA11 Semi-Flexible Grade Composition detail
Polymer 90 – 95 % Plasticizer/oil 5 – 10 %
PA11 Semi-Flexible Grade Physical properties
PA11 Semi-Flexible Grade Mechanical properties
Young’s modulus 0.44 – 0.52 GPa Specific stiffness 0.425 – 0.502 MN.m/kg Yield strength (elastic limit) 29 – 30 MPa Tensile strength 45 – 55 MPa Specific strength 28 – 29 kN.m/kg Elongation 360 % strain Elongation at yield 20 – 33 % strain Compressive modulus 0.44 – 0.52 GPa Compressive strength 54 – 66 MPa Flexural modulus 0.44 – 0.52 GPa Flexural strength (modulus of rupture) 42.1 – 43.5 MPa Shear modulus 0.16 – 0.18 GPa Shear strength 27 – 33 MPa Bulk modulus 0.78 – 1.13 GPa Poisson’s ratio 0.406 – 0.423 Shape factor 3.3 Hardness – Vickers 9 – 10 HV Hardness – Rockwell M 57 Hardness – Rockwell R 87 Hardness – Shore D 69 Elastic stored energy (springs) 832 – 995 kJ/m3 Fatigue strength at 10^7 cycles 18 – 22 MPa
PA11 Semi-Flexible Grade Impact & fracture properties
Fracture toughness 2.73 – 2.82 MPa.m0.5 Toughness (G) 14.7 – 17.6 kJ/m2 Impact strength, notched 23 °C 37 – 48 kJ/m2 Impact strength, notched -30 °C 7 – 10 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PA11 Semi-Flexible Grade Thermal properties
Melting point 187 – 189 °C Glass temperature 45 °C Heat deflection temperature 0.45MPa 135 °C Heat deflection temperature 1.8MPa 40 – 47 °C Vicat softening point 145 – 146 °C Maximum service temperature 90 – 105 °C Minimum service temperature -60 – -40 °C Thermal conductivity 0.19 – 0.29 W/m.°C Specific heat capacity 1730 – 1770 J/kg.°C Thermal expansion coefficient 138 µstrain/°C Thermal shock resistance 410 – 487 °C Thermal distortion resistance 0.00138 – 0.0021 MW/m Latent heat of fusion 39 kJ/kg
PA11 Semi-Flexible Grade Electrical properties
Electrical resistivity 1e18 µohm.cm Electrical conductivity 1.72e-16 %IACS Dielectric constant (relative permittivity) 4.2 – 5.92 Dissipation factor (dielectric loss tangent) 0.0473 – 0.125 Dielectric strength (dielectric breakdown) 24 – 26 MV/m Comparative tracking index 600 V
PA11 Semi-Flexible Grade Magnetic properties
Magnetic type Non-magnetic
PA11 Semi-Flexible Grade Optical, aesthetic and acoustic properties
Refractive index 1.51 – 1.53 Transparency Translucent Acoustic velocity 651 – 709 m/s Mechanical loss coefficient (tan delta) 0.0367 – 0.0399
PA11 Semi-Flexible Grade Absorption & permeability
Water absorption @ 24 hrs 0.3 % Water absorption @ sat 1.8 % Humidity absorption @ sat 0.9 % Water vapor transmission 0.39 g.mm/m².day Permeability (O2) 16.2 cm³.mm/m².day.atm
PA11 Semi-Flexible Grade Processing properties
Polymer injection molding Excellent Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1 – 2 % Melt temperature 260 – 270 °C Mold temperature 50 °C Molding pressure range 16 – 70 MPa
PA11 Semi-Flexible Grade Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Limited use Organic solvents Acceptable Oils and fuels Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA11 Semi-Flexible Grade Notes
PA11 Semi-Flexible Grade Other notes PA type 11 is not petroleum-based, but uses C11 derivatives of castor oil (a vegetable oil extracted from castor seeds) as its main chemical feedstock.
PA11 Grades
PA11 Unfilled Material Data Sheets
Other PA11 grades:
All PA11 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey