PA11 Unfilled Grades

PA11 Unfilled Grades

PA11 Unfilled Grades Overview

PA11 unfilled grades are polyamide 11 (nylon 11) compounds grouped by their reinforcement and additives. Unfilled grades contain no reinforcing fibers or mineral fillers, although some include lubricants, impact modifiers or flame retardants. They give the toughest, most ductile and easiest-to-machine form of the polymer, with good wear and sliding behaviour. The PA11 unfilled material data sheets below list designation, composition, physical, mechanical, thermal and electrical properties for each grade. Looking for PA11 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA11 parts in-house and inspects them before shipment.

PA11 Unfilled Material Data Sheets

PA11 Flexible Grade Material Data Sheet

PA11 Rigid Grade Material Data Sheet

PA11 Semi-Flexible Grade Material Data Sheet

More PA11 Grades

All PA11 grades