PA11 (nylon 11) absorbs little water and has reasonable UV resistance for a polyamide. It is more flexible and impact resistant than PA6 or PA66, and apart from PA12 it melts and processes at lower temperatures than the other grades. It is made from a renewable feedstock, castor bean oil.
PA11 Limitations
It is relatively expensive, and apart from PA12 its strength is the lowest of the polyamides.
Typical Uses of PA11
Hoses for air, hydraulic fluid or petrol, gears, cams, tool handles and powder coatings for metals.
PA11 Compositional Summary
(NH(CH2)10-CO)n. The renewable content comes from castor oil.
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PA11 (Polyamide / nylon 11)
CAS number
25035-04-5
PA11 Processing Properties
Feedstocks and Production
Based on C11 derivatives of castor oil rather than petroleum.
Forming
Molding temperatures are low for a polyamide.
Machining
It usually machines easily, although flexible grades are harder to machine.
Joining
Flexible grades are very difficult or impossible to weld ultrasonically.
PA11 Parts from Turkey
Looking for PA11 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA11 parts in-house and inspects them before shipment.