Thermal properties: HASTELLOY C-276 (Nickel-Mo-Cr alloy)
| Thermal properties: HASTELLOY C-276 (Nickel-Mo-Cr alloy) | |
| Melting point | 1330 – 1370 °C |
| Maximum service temperature | 910 – 1040 °C |
| Minimum service temperature | -273 °C |
| Thermal conductivity | 9.5 – 11.5 W/m.°C |
| Specific heat capacity | 420 – 435 J/kg.°C |
| Thermal expansion coefficient | 10 – 12 µstrain/°C |
| Thermal shock resistance | 136 – 186 °C |
| Thermal distortion resistance | 0.838 – 1.09 MW/m |
| Latent heat of fusion | 280 – 300 kJ/kg |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey