HASTELLOY C-276 Chemical Composition Summary (Nickel-Mo-Cr alloy)

Chemical Composition Summary : HASTELLOY C-276 (Nickel-Mo-Cr alloy)

Compositional summary
Ni51-64 / Mo15-17 / Cr14-16 / Fe4-7 / W3-4.5
(impurities: Co<2.5, Mn<1, V<0.35, Si<0.08, P<0.04, S<0.03, C<0.01)
Material family                                                                                       Metal (non-ferrous)
Base material                                                                                       Ni (Nickel)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey