Processing properties: HASTELLOY C-276 (Nickel-Mo-Cr alloy)
| Processing properties: HASTELLOY C-276 (Nickel-Mo-Cr alloy) | |
| Metal casting | Unsuitable |
| Metal cold forming | Excellent |
| Metal hot forming | Excellent |
| Metal press forming | Excellent |
| Metal deep drawing | Unsuitable |
| Machining speed | 4.88 m/min |
| Weldability | Excellent Notes: Preheating and post weld heat treatments are not required |
| Weldability – MIG | Good |
| Weldability – plasma | Good |
| Weldability – SAW | Not recommended |
| Weldability – TIG | Good |
| Brazeability | Good |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey