Chemical Composition Detail : HASTELLOY C-276 (Nickel-Mo-Cr alloy)
| HASTELLOY C-276 Composition detail | ||||
| C (carbon) | 0 | – | 0.01 | % |
| Co (cobalt) | 0 | – | 2.5 | % |
| Cr (chromium) | 14.5 | – | 16.5 | % |
| Fe (iron) | 4 | – | 7 | % |
| Mn (manganese) | 0 | – | 1 | % |
| Mo (molybdenum) | 15 | – | 17 | % |
| Ni (nickel) | 51 | – | 63.5 | % |
| P (phosphorus) | 0 | – | 0.04 | % |
| S (sulfur) | 0 | – | 0.03 | % |
| Si (silicon) | 0 | – | 0.08 | % |
| V (vanadium) | 0 | – | 0.35 | % |
| W (tungsten) | 3 | – | 4.5 | % |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey