International:
NiMo16Cr15Fe6W4 to ISO 6207, NiMo16Cr15Fe6W4 to ISO 6208, NiMo16Cr15Fe6W4 to ISO 9723, NiMo16Cr15Fe6W4 to ISO 9724, NiMo16Cr15Fe6W4 to ISO 9725, NW0276 to ISO 6207, NW0276 to ISO 6208, NW0276 to ISO 9723, NW0276 to ISO 9724, NW0276 to ISO 9725
Japan:
DNiCrMo-4 to JIS Z3224, NW0276 to JIS H4551, NW0276 to JIS H4552, NW0276 to JIS H4553, NW0276 to JIS H4554, YNiCrMo-4 to JIS Z3334
UK:
NA48 to BS 2901/5
USA:
ENiCrMo-4 to AWS A5.11/A5.11M, ERNiCrMo-4 to AWS A5.14/A5.14M, N10276 to ASTM B564, N10276 to ASTM B574, N10276 to ASTM B575, N10276 to ASTM B619, N10276 to ASTM B622, N10276 to ASTM B626, Ni 276 to ASTM F467M, Ni 276 to ASTM F468M, UNS N10276

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey