Designation: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)
ConditionAnnealed
UNS numberN06022
US nameASTM Grade N06022
EN nameNiCr21Mo14W
EN number2.4602
ISO nameISO 9723, 9724, 6207

Thermal properties: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)

Melting point1080–1130°C
Maximum service temperature910–1040°C
Minimum service temperature-273  °C
Thermal conductivity9.27–9.99W/m.°C
Specific heat capacity407–421J/kg.°C
Thermal expansion coefficient12.4  µstrain/°C
Thermal shock resistance121–149°C
Thermal distortion resistance0.747–0.805MW/m
Latent heat of fusion259–314kJ/kg

Electrical properties

Electrical resistivity112–116µohm.cm
Electrical conductivity1.48–1.54%IACS
Galvanic potential-0.14–-0.06V

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey