Designation: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)
ConditionAnnealed
UNS numberN06022
US nameASTM Grade N06022
EN nameNiCr21Mo14W
EN number2.4602
ISO nameISO 9723, 9724, 6207

Composition detail: HASTELLOY C-22 annealed

C (carbon)0–0.015%
Co (cobalt)0–2.5%
Cr (chromium)20–22.5%
Fe (iron)2–6%
Mn (manganese)0–0.5%
Mo (molybdenum)12.5–14.5%
Ni (nickel)50–63%
P (phosphorus)0–0.02%
S (sulfur)0–0.02%
Si (silicon)0–0.08%
V (vanadium)0–0.35%
W (tungsten)2.5–3.5%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey