HASTELLOY C-22 annealed Processing Properties (Nickel-Mo-Cr alloy)

Designation: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy) Condition Annealed UNS number N06022 US name ASTM Grade N06022 EN name NiCr21Mo14W EN number 2.4602 ISO name ISO 9723, 9724, 6207 Processing properties: HASTELLOY C-22 annealed Metal casting Unsuitable Metal cold forming Limited use Metal hot forming Acceptable Metal press forming Excellent Metal deep drawing Unsuitable Machining speed … Continue reading HASTELLOY C-22 annealed Processing Properties (Nickel-Mo-Cr alloy)