HASTELLOY C-22 annealed Equivalent Grades (Nickel-Mo-Cr alloy)

Designation: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)
ConditionAnnealed
UNS numberN06022
US nameASTM Grade N06022
EN nameNiCr21Mo14W
EN number2.4602
ISO nameISO 9723, 9724, 6207
Tradenames: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)
INCONEL 22, Special Metals Corp. (USA)

Equivalent / Similar compositions: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy)

International: NiCr21Mo13Fe4W3 to ISO 6207, NiCr21Mo13Fe4W3 to ISO 6208, NiCr21Mo13Fe4W3 to ISO 9723, NiCr21Mo13Fe4W3 to ISO 9724, NW6022 to ISO 6207, NW6022 to ISO 6208, NW6022 to ISO 9723, NW6022 to ISO 9724
Japan: NW6022 to JIS H4551, NW6022 to JIS H4552, NW6022 to JIS H4553, NW6022 to JIS H4554
USA: ENiCrMo-10 to AWS A5.11/A5.11M, ERNiCrMo-10 to AWS A5.14/A5.14M, N06022 to ASTM B564, N06022 to ASTM B574, N06022 to ASTM B575, N06022 to ASTM B619, N06022 to ASTM B622, N06022 to ASTM B626, UNS N06022
Tradenames: INCONEL FILLER METAL 622, INCONEL WELDING ELECTRODE 122, NAS NW22, NICROFER 5621HMOW-ALLOY 22, NICROFER B 5621-FM 22, NICROFER S 5621-FM 22

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey