HASTELLOY C-22 annealed Equivalent Grades (Nickel-Mo-Cr alloy)

Designation: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy) Condition Annealed UNS number N06022 US name ASTM Grade N06022 EN name NiCr21Mo14W EN number 2.4602 ISO name ISO 9723, 9724, 6207 Tradenames: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy) INCONEL 22, Special Metals Corp. (USA) Equivalent / Similar compositions: HASTELLOY C-22, annealed (Nickel-Mo-Cr alloy) International: NiCr21Mo13Fe4W3 to ISO 6207, NiCr21Mo13Fe4W3 … Continue reading HASTELLOY C-22 annealed Equivalent Grades (Nickel-Mo-Cr alloy)