| Designation | |
| UNS number | N10665 |
| US name | ASTM Grade N10655 |
| EN number | 2.4617 |
Thermal properties: HASTELLOY B-2
| Melting point | 1350 | – | 1400 | °C |
| Maximum service temperature | 540 | – | 815 | °C |
| Minimum service temperature | -273 | °C | ||
| Thermal conductivity | 10 | – | 12.5 | W/m.°C |
| Specific heat capacity | 365 | – | 380 | J/kg.°C |
| Thermal expansion coefficient | 9.5 | – | 11.5 | µstrain/°C |
| Thermal shock resistance | 156 | – | 238 | °C |
| Thermal distortion resistance | 0.926 | – | 1.24 | MW/m |
| Latent heat of fusion | 285 | – | 300 | kJ/kg |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey