HASTELLOY B-2 Equivalent Grades (plate, Nickel-molybdenum alloy)

General information

Designation
UNS numberN10665
US nameASTM Grade N10655
EN number2.4617

Tradenames: HASTELLOY B-2, Haynes International Inc. (USA)

Equivalent Grades / Similar compositions: HASTELLOY B-2

International: NiMo28 to ISO 6207, NiMo28 to ISO 6208, NiMo28 to ISO 9723, NiMo28 to ISO 9724, NiMo28 to ISO 9725, NW0665 to ISO 6207, NW0665 to ISO 6208, NW0665 to ISO 9723, NW0665 to ISO 9724, NW0665 to ISO 9725
Japan: NW0665 to JIS H4551, NW0665 to JIS H4552, NW0665 to JIS H4553, NW0665 to JIS H4554
USA: N10665 to ASTM B333, N10665 to ASTM B335, N10665 to ASTM B564, N10665 to ASTM B619, N10665 to ASTM B622, N10665 to ASTM B626, UNS N10665
Tradenames: ERGILOY 4617 HH, HASTELLOY ALLOY B-2, NICROFER B 6928 – WS B-2, NIMOFER S 6928-FM B-2

Typical uses: Chemical processing, esp. handling of hydrochloric acid, high temperature applications where a low coefficient of expansion is required.

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey