HASTELLOY B-2 Mechanical Properties (plate, Nickel-molybdenum alloy)
Designation UNS number N10665 US name ASTM Grade N10655 EN number 2.4617 Mechanical properties: HASTELLOY B-2, plate Young’s modulus 209 – 223 GPa Specific stiffness 22.6 – 24.2 MN.m/kg Yield strength (elastic limit) 360 – 525 MPa Tensile strength 805 – 995 MPa Specific strength 39 – 56.9 kN.m/kg Elongation 50 – 70 % strain … Continue reading HASTELLOY B-2 Mechanical Properties (plate, Nickel-molybdenum alloy)