HASTELLOY B-2 Durability and Corrosion Resistance (plate, Nickel-molybdenum alloy)

Designation
UNS numberN10665
US nameASTM Grade N10655
EN number2.4617

Durability: HASTELLOY B-2

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsExcellent
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500°CExcellent
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)
Notes :Bronze or zinc alloy dies should be used to minimize galling.
Limited use
FlammabilityNon-flammable

Corrosion resistance: HASTELLOY B-2

Stress corrosion cracking
Note:
Slightly susceptible
Rated in chloride; Other susceptible environments: Hydroxide
Intergranular (weld line) corrosionExcellent
Inorganic acidsExcellent
Organic acidsGood
AlkalisExcellent
Humidity / waterExcellent
Sea waterExcellent
Sour oil and gasExcellent

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey