| Designation | |
| UNS number | N10665 |
| US name | ASTM Grade N10655 |
| EN number | 2.4617 |
Composition: HASTELLOY B-2
| C (carbon) | 0 | – | 0.02 | % |
| Co (cobalt) | 0 | – | 1 | % |
| Cr (chromium) | 0 | – | 1 | % |
| Fe (iron) | 0 | – | 2 | % |
| Mn (manganese) | 0 | – | 1 | % |
| Mo (molybdenum) | 26 | – | 30 | % |
| Ni (nickel) | 64.8 | – | 74 | % |
| P (phosphorus) | 0 | – | 0.04 | % |
| S (sulfur) | 0 | – | 0.03 | % |
| Si (silicon) | 0 | – | 0.1 | % |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey