Bronze CuAl10Fe5Ni5 Chemical Composition (C95820, cast aluminum bronze)

Designation
CuAl10Fe5Ni5
UNS numberC95820
EN nameCC333G
ISO nameCuAl10Fe5Ni4
GB (Chinese) nameCuAl9Fe4Ni4Mn2
JIS (Japanese) nameAl BC 3

Bronze CuAl10Fe5Ni5 Chemical Composition (C95820, cast aluminum bronze)

Al (aluminum)9–10%
Cu (copper)77.4–82.5%
Fe (iron)4–5%
Mn (manganese)0–1.5%
Ni (nickel)4.5–5.8%
Pb (lead)0–0.02%
Si (silicon)0–0.1%
Sn (tin)0–0.02%
Zn (zinc)0–0.2%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey