Bronze CuAl10Fe5Ni5 Similar Compositions (C95820, cast aluminum bronze)

Designation
CuAl10Fe5Ni5
UNS numberC95820
EN nameCC333G
ISO nameCuAl10Fe5Ni4
GB (Chinese) nameCuAl9Fe4Ni4Mn2
JIS (Japanese) nameAl BC 3

Bronze CuAl10Fe5Ni5 Equivalent Grades (C95820, cast aluminum bronze)

Europe: CB333G to CEN EN 1982, CC333G to CEN EN 1982
Germany: 2.0976 to DIN 17656, GB-CuAl10Ni to DIN 17656
International: CuAl10Fe5Ni5 to ISO 1637, CuAl10Fe5Ni5 to ISO 1640, CuAl10Fe5Ni5 to ISO 4382-1
Japan: AlBC3 to JIS H5114, CAC703 to JIS H5120, CAC703C to JIS H5121
Sweden: 5716-03 to SIS 145716, 5716-06 to SIS 145716, 5716-15 to SIS 145716
UK: HC502 to BS HC502
USA: C95820, C95820 to ASTM B148, UNS C95820
Tradenames: KRAMER N ALUMINUM BRONZE, LILY BRAND NO. 15, MTEK 230-N, TAB-5 N1

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey