Bronze CuAl10Fe5Ni5 Mechanical Properties (C95820, cast aluminum bronze)

Designation CuAl10Fe5Ni5 UNS number C95820 EN name CC333G ISO name CuAl10Fe5Ni4 GB (Chinese) name CuAl9Fe4Ni4Mn2 JIS (Japanese) name Al BC 3 Bronze CuAl10Fe5Ni5 Mechanical Properties (C95820, cast aluminum bronze) Young’s modulus 110 – 113 GPa Specific stiffness 14.2 – 15.2 MN.m/kg Yield strength (elastic limit) 250 – 300 MPa Tensile strength 640 – 700 MPa … Continue reading Bronze CuAl10Fe5Ni5 Mechanical Properties (C95820, cast aluminum bronze)