Bronze CuAl10Fe5Ni5 Similar Compositions (C95820, cast aluminum bronze)

Designation CuAl10Fe5Ni5 UNS number C95820 EN name CC333G ISO name CuAl10Fe5Ni4 GB (Chinese) name CuAl9Fe4Ni4Mn2 JIS (Japanese) name Al BC 3 Bronze CuAl10Fe5Ni5 Equivalent Grades (C95820, cast aluminum bronze) Europe: CB333G to CEN EN 1982, CC333G to CEN EN 1982 Germany: 2.0976 to DIN 17656, GB-CuAl10Ni to DIN 17656 International: CuAl10Fe5Ni5 to ISO 1637, CuAl10Fe5Ni5 … Continue reading Bronze CuAl10Fe5Ni5 Similar Compositions (C95820, cast aluminum bronze)