| Designation | |
| 6060, wrought | |
| UNS number | A96060 |
| EN name | EN AW-6060 (EN AW-Al MgSi) |
| EN number | 3.3206 |
Aluminum 6060 Equivalent Grades
| Australia: 6060 to AS 2848.1, 6101 to AS 2848.1 |
| Austria: AlMgSi0.5 to ONORM M3430, E-AlMgSi to ONORM M3430 |
| Canada: 0.606 to CSA HA.5 |
| Europe: EN AW-6060 to CEN EN 573-3, EN AW-6101 to CEN EN 573-3 |
| France: 6060 to NF A50-411, 6060 to NF A50-701 |
| Germany: 3.2305/E-AlMgSi to DIN 1725-1, 3.3206/AlMgSi0.5 to DIN 1725-1, 3.3207/E-AlMgSi0.5 to DIN 1725-1 |
| International: AlMgSi to ISO 209-1, EAlMgSi to ISO 209-1 |
| Japan: A6101PB to JIS H4180, A6101SB to JIS H4180, A6101SBC to JIS H4180, A6101TB to JIS H4180 |
| Norway: 17301 to NS 17301, 17302 to NS 17302 |
| Sweden: 4103 to MNC 40E, 4103-00 to SIS 144103, 4103-04 to SIS 144103, 4103-06 to SIS 144103 |
| UK: 6060 to BS 1474 |
| USA: 6060, 6060 to ASTM B221M, 6101, 6101 to ASTM B317, 6101B, UNS A96060, UNS A96101 |
| Yugoslavia: 3.5452.00/AlMgSi0.5 to JUS C.C2.100, 3.5453.00/AlMgSiE to JUS C.C2.100, 3.5454.00/AlMgSi0.5E to JUS C.C2.100 |
| Tradenames: AL99.85MGSI0.4 (481) 6032, ALMGSI0.3 (466) 6030, ALMGSI0.5 (461) 6040, BALCO ALLOY 6063.20, BALCO ALLOY 6063.30, E-ALMGSI 0.5 (491) 6047, RAPIDEX-040, RAPIDEX-041, RAPIDEX-043, RAPIDEX-050, RAPIDEX-051 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey