Aluminum 6060 T4 Mechanical Properties

Designation 6060, wrought Condition T4  (Solution heat-treated and naturally aged to a substantially stable condition) UNS number A96060 EN name EN AW-6060 (EN AW-Al MgSi) EN number 3.3206 Aluminum 6060 T4 Mechanical Properties Young’s modulus 69.5 – 73 GPa Specific stiffness 25.7 – 27.1 MN.m/kg Yield strength (elastic limit) 60 – 70 MPa Tensile strength … Continue reading Aluminum 6060 T4 Mechanical Properties