Aluminum 6060 T6 Mechanical Properties
Designation 6060, wrought Condition T6 (Solution heat-treated and artificially aged) UNS number A96060 EN name EN AW-6060 (EN AW-Al MgSi) EN number 3.3206 Aluminum 6060 T6 Mechanical Properties Young’s modulus 69.5 – 73 GPa Specific stiffness 25.6 – 26.9 MN.m/kg Yield strength (elastic limit) 150 – 175 MPa Tensile strength 190 – 222 MPa Specific … Continue reading Aluminum 6060 T6 Mechanical Properties