Aluminum 6060 Chemical Composition
Designation 6060, wrought UNS number A96060 EN name EN AW-6060 (EN AW-Al MgSi) EN number 3.3206 Aluminum 6060 Chemical Composition Al (aluminum) 97.8 – 99.2 % Cr (chromium) 0 – 0.05 % Cu (copper) 0 – 0.1 % Fe (iron) 0.1 – 0.3 % Mg (magnesium) 0.35 – 0.6 % Mn (manganese) 0 – 0.1 … Continue reading Aluminum 6060 Chemical Composition